2012/8/15      view:

Grade / fairly standard ISO / physical and mechanical properties (min): Bending strength N / mm2; hardness HRA

 / uses. 

1, YG3x / K01 / 1420; 92.5 / for cast iron, nonferrous metals and alloys, low alloy steel, hardened steel cutting 

cross-section high-speed finishing. 

2, YG6 / K20 /1900;90.5/ for cast iron, nonferrous metals and alloys, non-metallic materials until the next semi-finishing and finishing cutting speed. 

3, YG6x / K15 / 1800; 92.0 / suitable for chilled cast iron, ductile iron, gray iron, heat-resistant alloy steel cutting small section of high-speed finishing, semi-finishing. 

4, YG6A / K10 / 1800; 92.0 / suitable for chilled cast iron, ductile iron, gray iron, the small section of heat-resistant alloys, high-speed cutting finishing. 

5, YG8 / K30 / 2200; 90.0 / for cast iron, nonferrous metals and alloys, non-metallic materials low speed roughing. 

6, YG8N / K30 / 2100; 90.5 / for cast iron, white cast iron, ductile iron and chrome-nickel stainless steel and other alloy materials, high-speed cutting. 

7, YG15 / K40 / 2500; 87.0 / inlay system suitable for oil wells, coal mining drill, geological exploration drill. 

8, YG4C / 1600; 89.5 / inlay system suitable for oil wells, coal mining drill, geological exploration drill. 

9, YG8C / 1800; 88.5 / inlay system suitable for oil, mining drill bit word, cross bits, roller cone drill teeth, DTH 

drilling teeth. 

10, YG11C / 2200; 87.0 / inlay system suitable for oil, mining drill bit word, cross bits, roller cone drill teeth, DTH

 drilling teeth. 

11, YW1 / M10 / 1400; 92.0 / suitable for steel, heat resistant steel, high manganese steel and cast iron semi-finishing speed. 

12, YW2 / M20 / 1600; 91.0 / suitable for heat-resistant steel, high manganese steel, stainless steel and other difficult to 

machine steels, low-speed roughing and semi-finishing.